PSI - Issue 37
Aleksandar Sedmak et al. / Procedia Structural Integrity 37 (2022) 263–268 Author name / Structural Integrity Procedia 00 (2019) 000 – 000
267
5
a)
b)
Fig. 5. Regular regime (a) Loading; (b) Stress contours
a)
b)
Fig. 6. Irregular regime (a) Loading; (b) Stress contours
4. Conclusions Based on the results presented in this paper, one can conclude the following: • Minimum critical crack length value is far above the length of detected cracks (146 vs. 25 mm), so there is no danger of brittle fracture. • High cycle fatigue amplitude stress is far below values that should be considered for further analysis • Low cycle fatigue amplitude stress is not enough to reduce cover working life since it happens only 2000 times per year. Acknowledgements This research was supported by the Ministry of Sciences and Technology of Republic of Serbia through the contracts 451-03-9/2021-14/200105 and 451-03-9/2021-14/200213.
Made with FlippingBook Ebook Creator