PSI - Issue 2_B
L. Esposito / Procedia Structural Integrity 2 (2016) 919–926
924 6
L. Esposito/ Structural Integrity Procedia 00 (2016) 000–000
Fig. 4: Effect of the grain size on the minimum creep rate.
Fig. 5: Localization of creep strain due to the fine grain, (50MPa simulation).
Fig. 6: Failure onset in FGHAZ without necking, (50MPa simulation).