PSI - Issue 14

Vikas Verma et al. / Procedia Structural Integrity 14 (2019) 68–77 Author name / Structural Integrity Procedia 00 (2018) 000 – 000

75

8

Fig. 6. SEM images of (a) pure Al alloy wear at 15 N (b) pure Al alloy wear at 25 N (c) Al alloy +5%Fly ash +6%Al 2 O 3 wear at 25 N (d) Al Alloy+5%Fly ash+9%Al 2 O 3 wear at 25 N (e) Al Alloy+5%Fly ash+12%Al 2 O 3 wear at 15 N (f) Al Alloy+5%Fly ash+12%Al 2 O 3 wear at 25 N