PSI - Issue 66

S. Skrobacz et al. / Procedia Structural Integrity 66 (2024) 11–25 S. Skrobacz¹², P. Krysi ń ski¹, S. Ma ł ys¹², T. Ł agoda², / Structural Integrity Procedia 00 (2025) 000–000

19

9

Table 5. Description of 2HY Joint for Sample PR-908 - Sketch of the Sample, Notes, and Detected Defects

Welding Position/Method

Type of Joint

Type of Weld

Filler Material

Shielding Gas

BW

2HY

PA

131(robot)

AlMg4.5MnZr

I1 (Ar100%)

Sketch of the Sample

1: 504; h ₘ ₐₓ =3.0mm; h ₐ ≤ 4.0mm 2: 504 h ₘ ₐₓ =1.8mm; h ₐ ≤ 4.0mm

Notes, and Detected Defects

2/2

1/2

Figure 7. Macrographic Cross-Sections of Sample Number PR-908

Made with FlippingBook Ebook Creator