Issue 62
A. Brotzu et alii, Frattura ed Integrità Strutturale, 62 (2022) 64-74; DOI: 10.3221/IGF-ESIS.62.05
Figure 8: Typical guided bending test plot obtained on a not corroded specimen.
Figure 9: Cyclic guided bending test results on a corroded specimen ◆ deformation angle under load, ◼ deformation angle without load (elastic recovery) ▲ residual angle deformation after heating at 70 °C for 1 minute (shape memory recovery).
a) As corroded
b) 1° cycle, plunger shift 5 mm
c) 5°cycle, plunger shift 5 mm
71
Made with FlippingBook PDF to HTML5