Issue 62
M. Saltan et alii, Frattura ed Integrità Strutturale, 62 (2022) 54-63; DOI: 10.3221/IGF-ESIS.62.04
Sample
Penetration (25 ˚ C) Softening Point ( ˚ C)
Ductility (5cm/min)
Specific Gravity (g/cm 3 )
Reference
50
49.8
>100
1.021
1% CDEA
53
47.8
>100
1.028
3% CDEA
66
45.5
>100
1.015
5% CDEA
71
44.5
>100
1.022
Table 4: Results of conventional bitumen tests.
Figure 2: Graphs of reference bituminous binder.
Figure 3: Graphs of reference bituminous binder modified with 5% CDEA.
58