H. Guedaoura et alii, Frattura ed Integrità Strutturale, 62 (2021) 26-53; DOI: 10.3221/IGF-ESIS.62.03
Figure 20: Bond behavior of specimen B1-R2-6.
Figure 21: Bond behavior of specimen B1-R3-6.
GFRP laminates of 10 mm thicknesses When the thicknesses of the GFRP laminates were increased to 10 mm, very intriguing results were observed. In contrast to B1-U0, specimens B1-R1-10, B1-R2-10, B1-R3-10, and B1-R4-10 improved in strength by 37 %, 33 %, 23 %, and 45