Rando Tungga Dewa et al. / Procedia Structural Integrity 57 (2024) 762–771 Dewa et al./ Structural Integrity Procedia 00 (2019) 000 – 000

769

8

Fig. 7. SEM micrographs of fracture surface specimen tested at 1E-2 s-1, showing typical crack initiation, propagation, and failure zone features .