PSI - Issue 5
Ewelina Małek et al. / Procedia Structural Integrity 5 (2017) 508 – 515 Ewelina Małek / Structural Integrity Procedia 00 (2017) 000 – 000
514
7
4.2. Fireproof textile – Natan Test results has shown that the amount of heat radiation passed through the sample with TiSi coating was smaller than for the sample without coating. The example of that phenomenon was shown in Fig. 11.
a)
b)
Fig. 11. On the left – material without coating, on the right – material with coating
Test results for all Scenario for both samples (with coating and without coating) as temperature vs. time chart were in Fig. 12.
Fig. 12. Test results for all Scenario for both samples (with coating and without coating) as temperature vs. time chart)
5. Summary The conducted research has shown that temperature differences between textile with coating and without coating for both fabrics at the beginning and the end of the test were: for fireproof textile Proton
Scenario 1 - 60 °C: end of the test - 0,4°C Scenario 2 - 100 °C: end of the test - 1,03°C
Made with FlippingBook - Online catalogs