Andrzej Katunin et al. / Procedia Structural Integrity 5 (2017) 416–421 Andrzej Katunin/ Structural Integrity Procedia 00 (2017) 000 – 000
419
4
Fig. 2. Damage occurring after fatigue with self-heating observed when the maximal self-heating temperature values of a) 60°C, b) 70°C, c) 90°C, and d) 110°C were reached.