PSI - Issue 36
Ye. Kryzhanivskyy et al. / Procedia Structural Integrity 36 (2022) 370–377 Ye. I. Kryzhanivskyy et al. / Structural Integrity Procedia 00 (2021) 000 – 000
375
6
Fig. 2. Graphical dependences of pressure change in the pipeline at different pumping points of СО 2 : 1 – injection in a single point ( х п1 =0 m ); 2 – injection in two points ( х п1 =0 m , х п2 =1200 m ); 3 – injection in four points ( х п1 =0 m, х п2 =400 m, х п3 =800 m, х п4 =1200 m).
a)
b)
c)
Fig. 3. Graphical dependences of pressure change in time for different injection points СО 2 : a – injection in a single point; b – injection in two points; c – injection in four points.