O.B. Naimark et al. / Procedia Structural Integrity 33 (2021) 1115–1122 Naimark O.B. et al / Structural Integrity Procedia 00 (2021) 000–000

1120

6

Fig. 5. Temporal scenario of strain components and corresponding phase portraits

3. Results and discussion

Duality of criticality of damage-failure transitions, caused by two intermediate self-similar singular solutions for the stress field at the crack tip and blow-up damage localization kinetics, is used for the interpretation of two-parameters