Alok Gupta et al. / Procedia Structural Integrity 31 (2021) 15–21 Alok Gupta et al. / Structural Integrity Procedia 00 (2019) 000–000
20
6
(b)
(a)
Fig. 5. (a) FRC in the axial direction showing the fundamental vibration mode at 84 Hz, (b) FRC in the tangential direction with distinct peaks at 84Hz and 183Hz (the second vibration mode).
5
3
1
4
2
Location 1
Fig. 6. SLM bracket after dwell test with numbers indicating the sequence and location of fracture, picture in the inset shows a magnified view of the first fracture in the middle diagonal strut
Location 1
(a)
(b)
Location 1
Crack Initiation
Beach Marks
Crack Propagation Direction
200 m
50 m
Fig. 7. (a) SEM micrograph showing crack initiation site of location 1 and direction of crack propagation, (b) SEM micrograph showing magnified view with beach marks at location 1