F. Berto et al. / Procedia Structural Integrity 3 (2017) 77–84 F. Berto et al./ Structural Integrity Procedia 00 (2017) 000–000

82

6

a

b

Fig. 5. Typical fracture surface after cyclic loading. (a) Plate and (b) bolted part.

Fig. 6. Layer thickness from a SEM image.

Fig. 7. S-N-curves of hot dip galvanized connections.