grain size in the zones obtained at stationary welding (average grain diameter - 4.50 microns), i.e. structure grinding set by 18%.
Fig. 4. Comparison of the sizes of the HAZ at temperatures of 21 0 C (red line) and - 42 0 C (blue line).
a
b
c
d
Fig. 5. The structure of the HAZ (x100): a) adaptive pulse-arc mode at t = + 21 0 C, b) a stationary mode when t = + 21 0 C, c) adaptive pulse-arc mode at t = - 42 0 C, d) a stationary mode when t = - 42 0 C.