F. Moroni et al. / Procedia Structural Integrity 18 (2019) 516–524 F. Moroni / Structural Integrity Procedia 00 (2019) 000–000

520

5

Figure 3. Example of secondary delamination in a DCB test (T1100_03 specimen).

(a)

(b)

Figure 4. Mode I R-curve of: (a) T1100+2573 resin; (b) T700+ER450 resin co-laminated DCB tests.

(a)

(b)

Figure 5. Example of force vs. opening behavior and fracture surface of: (a) T1100+2573 resin; (b) T700+ER450 resin co-laminated ENF tests.