PSI - Issue 14

K. Chawla et al. / Procedia Structural Integrity 14 (2019) 571–576 K.Chawla et al. Structural Integrity Procedia 00 (2018) 000 – 000

576

6

nanofiber interlayer. Composites Science and Technology , 68:516 – 525, Dong, W., Liu, H. C., Park, S. J., Jin., F. L., 2014. Fracture toughness improvement of epoxy resins with short carbon fibers. Journal of Industrial and Engineering Chemistry , 2014. Yesgat, A. L., Kitey., R., 2016. Effect of filler geometry on fracture mechanisms in glass particle filled epoxy composites. Engineering Fracture Mechanics , 160:22 – 41, 2016. ASTM D5528-13. Standard test method for Mode I interlaminar fracture toughness of unidirectional fiber-reinforced polymer matrix composites.

Made with FlippingBook Annual report maker