Issue 59
A. Houari et alii, Frattura ed Integrità Strutturale, 59 (2022) 212-231; DOI: 10.3221/IGF-ESIS.59.16
Figure 12: The variation of axial stress according to the thickness for the three positions of the defect (with ratio of radius ex in R / R constant and n kept constant=0.65).
Figure 13: Equivalent plastic strain distribution in FGM cylinder (n=0.65)
In Fig.12, the axial stresses are clearly affected by the presence and location of defects that amplify the level and distribution of stresses. The peaks of the stresses explain the compression in the form of elongation in a direction slightly
226
Made with FlippingBook Digital Publishing Software