Issue56

A. G. Joshi et alii, Frattura ed Integrità Strutturale, 56 (2021) 65-73; DOI: 10.3221/IGF-ESIS.56.05

Figure 1: Schematic diagram of different worn region in abrasive wear

Figure 2: SEM image of unfilled GE composite upside region (a) Low magnification, (b) Moderate magnification, (c) High magnification.

Figure 3: SEM image of unfilled GE composite central region (a) Low magnification, (b) Moderate magnification, (c) High magnification.

Figure 4: SEM image of unfilled GE composite bottom region (a) Low magnification, (b) Moderate magnification, (c) High magnification

70

Made with FlippingBook PDF to HTML5