Issue56

K. Fawzy et al, Frattura ed Integrità Strutturale, 56 (2021) 123-136; DOI: 10.3221/IGF-ESIS.56.10

Strengthening schemes

Beam No.

Type of strengthening

Control beam

B 00

B 01

One layer with length 1700 mm

two layers with length 1700 & 1400 mm

B 02

three layers with length 1700 & 1400 & 1100 mm

B 03

One layer and on sides above bottom edge by 20 mm with length 1700 mm

B 04

B 05

One layer and 6 U shapes

B 06

two layers and 6 U shape

B 07

Three layers and 6-U shape

One layer with length 1700 mm with lower longitudinal reinforcement 16 mm diameter One layer with length 1700 mm with lower longitudinal reinforcement 12 mm diameter

B 08

B 09

Table 4. Strengthening scheme.

Deflection and failure modes The mechanisms of failure can be categorized in global failure and local failure [13-15].  global failure involves compression failure of concrete in bending before or after yielding of steel, rupture of FRP layer in tension, and shear failure of concrete.

127

Made with FlippingBook PDF to HTML5