PSI - Issue 83
Ahmad Issmail et al. / Procedia Structural Integrity 83 (2026) 229–238
238
[14] L. C. Araújo et al. , “Effects of build orientation and heat treatments on the tensile and fracture toughness properties of additively manufactured AlSi10Mg,” Int. J. Mech. Sci. , vol. 213, p. 106868, Jan. 2022, doi: 10.1016/j.ijmecsci.2021.106868. [15] N. T. Aboulkhair, I. Maskery, C. Tuck, I. Ashcroft, and N. M. Everitt, “The microstructure and mechanical properties of selectively laser melted AlSi10Mg: The effect of a conventional T6-like heat treatment,” Mater. Sci. Eng. A , vol. 667, pp. 139–146, Jun. 2016, doi: 10.1016/j.msea.2016.04.092. [16] A. Issmail and N. Razavi, “Miniaturization Effects and Orientation–Size Interplay in the Fatigue Behaviour of LPBF AlSi10Mg,” Submitted to FFEMS for pubblication - Under Review . [17] “EOS GmbH, 2022. EOS Aluminum AlSi10Mg Datasheet. EOS GmbH, Krailling, Germany. https://www.eos.info/en/materials/aluminum-alsi10mg.” [18] N. Takata, H. Kodaira, K. Sekizawa, A. Suzuki, and M. Kobashi, “Change in microstructure of selectively laser melted AlSi10Mg alloy with heat treatments,” Mater. Sci. Eng. A , vol. 704, pp. 218–228, Sep. 2017, doi: 10.1016/j.msea.2017.08.029. [19] F. Del Re et al. , “Mechanical properties characterisation of AlSi10Mg parts produced by laser powder bed fusion additive manufacturing,” Int. J. Mater. Res. , vol. 110, no. 5, pp. 436–446, May 2019, doi: 10.3139/146.111761. [20] T. Maconachie et al. , “Effect of build orientation on the quasi-static and dynamic response of SLM AlSi10Mg,” Mater. Sci. Eng. A , vol. 788, p. 139445, Jun. 2020, doi: 10.1016/j.msea.2020.139445. [21] Q. Pu et al. , “The Influence of Post-Treatment on Micropore Evolution and Mechanical Performance in AlSi10Mg Alloy Manufactured by Laser Powder Bed Fusion,” Materials , vol. 17, no. 17, p. 4319, Aug. 2024, doi: 10.3390/ma17174319. [22] N. T. Aboulkhair, I. Maskery, C. Tuck, I. Ashcroft, and N. M. Everitt, “Improving the fatigue behaviour of a selectively laser melted aluminium alloy: Influence of heat treatment and surface quality,” Mater. Des. , vol. 104, pp. 174–182, Aug. 2016, doi: 10.1016/j.matdes.2016.05.041. [23] N. Razavi, S. Bagherifard, S. Hafnor, S. Spiller, M. Guagliano, and F. Berto, “Fatigue analysis of as-built and heat treated severely notched AlSi10Mg alloy specimens made by laser powder bed fusion technology,” Int. J. Fatigue , vol. 179, p. 108041, Feb. 2024, doi: 10.1016/j.ijfatigue.2023.108041. [24] K. Jamali Dogahe et al. , “Multiscale Study of the Fatigue Life of AlSi10Mg Material Produced by Laser Powder Bed Fusion (LPBF) Method: Experimental and Computational,” Fatigue Fract. Eng. Mater. Struct. , vol. 48, no. 5, pp. 2290–2308, May 2025, doi: 10.1111/ffe.14595. [25] H. Liu et al. , “Review on Fatigue of Additive Manufactured Metallic Alloys: Microstructure, Performance, Enhancement, and Assessment Methods,” Adv. Mater. , vol. 36, no. 17, p. 2306570, Apr. 2024, doi: 10.1002/adma.202306570. [26] J. N. Domfang Ngnekou et al. , “Fatigue properties of AlSi10Mg produced by Additive Layer Manufacturing,” Int. J. Fatigue , vol. 119, pp. 160–172, Feb. 2019, doi: 10.1016/j.ijfatigue.2018.09.029. [27] Z. Xu, A. Liu, and X. Wang, “Fatigue performance and crack propagation behavior of selective laser melted AlSi10Mg in 0°, 15°, 45° and 90° building directions,” Mater. Sci. Eng. A , vol. 812, p. 141141, Apr. 2021, doi: 10.1016/j.msea.2021.141141. [28] R. Molaei and A. Fatemi, “Crack paths in additive manufactured metallic materials subjected to multiaxial cyclic loads including surface roughness, HIP, and notch effects,” Int. J. Fatigue , vol. 124, pp. 558–570, Jul. 2019, doi: 10.1016/j.ijfatigue.2019.03.007.
Made with FlippingBook - Online catalogs