PSI - Issue 77
Jan Kec et al. / Procedia Structural Integrity 77 (2026) 264–271
270
(a)
(b)
Fig. 6. J-R curves for samples tested in air (a) and hydrogen charged (b)
(a)
(b)
Fig. 7. Fracture surfaces of stable crack growth of the sample tested in air (a) and hydrogen charged (b)
(a)
(b)
Fig. 8. Hydrogen effect on FCGR (a) and FT (b)