Issue 74

M. Bader et alii, Fracture and Structural Integrity, 74 (2025) 115-128; DOI: 10.3221/IGF-ESIS.74.08

Figure 7: Crack pattern of slab specimen SB-5-0.

Figure 8: Crack patterns in 50 mm void bubble slabs before CFRP rehabilitation and re-testing to failure: (a) SB-5 50, (b) SB-5-60, (c) SB-5-75.

Figure 9: Crack patterns in 50 mm void bubble slabs after CFRP rehabilitation and re-testing to failure: (a) SB-5-50, (b) SB-5-60, (c) SB 5-75.

121

Made with FlippingBook - professional solution for displaying marketing and sales documents online