Tapan K. Sawarn et al. / Procedia Structural Integrity 71 (2025) 263–270
267
(a)
(b)
(c)
Fig. 3. Typical appearances of the cladding tubes after 4PBT: Non-cracked (a) 1000°C & (b) 1100°C; Cracked from the burst opening tips (c) 1200°C.
Near Burst
Opposite to burst
1000°C
1000°C
Recrystallized Equiaxed α -Zr
Recrystallized equiaxed α -Zr
1100°C
1100°C
Recrystallized α -Zr
Prior β -Zr
Oxygen rich region
Oxide
1200°C