PSI - Issue 66
Sneha et al. / Procedia Structural Integrity 66 (2024) 419–425 Sneha, S.Ray/ Structural Integrity Procedia 00 (2025) 000–000
424
6
Figure 4. Fracture energy variation with different fibre combinations.
Figure 5. Variation of load from test machine vs crack length from the DIC
4. Conclusion This research investigated the effect of hybrid fibres with different fibre lengths and volume fractions on post cracking behaviour using fracture and non-destructive testing. The findings have been summarized below. Compressive strength of 126 MPa has been achieved with ultra-fine material and dense microstructure. The incorporation of 2% fibres demonstrates a more pronounced impact on both the peak load and post peak behaviour of the material.
Made with FlippingBook Ebook Creator