Figure 5. Macrographic Cross-Sections of Sample Number PR-906

Table 4. Description of 2Y Joint for Sample PR-907 - Sketch of the Sample, Notes, and Detected Defects

Welding Position/Method

Type of Joint

Type of Weld

Filler Material

Shielding Gas

BW

2Y

PA

131(robot)

AlMg4.5MnZr

I1 (Ar100%)

Sketch of the Sample

1: End with Gas Porosity; 2011; d ₘ ₐₓ = 0.1 mm; d ₐ ≤ 0.6mm 2: 504; h ₘ ₐₓ = 1.8 mm; h ₐ ≤ 3.0mm 3: 504; h ₘ ₐₓ = 3.2 mm; h ₐ ≤ 3.0mm

Notes, and Detected Defects