Issue 66

M. Sánchez et alii, Frattura ed Integrità Strutturale, 66 (2023) 322-338; DOI: 10.3221/IGF-ESIS.66.20

 12 PLA plates with W=60 mm, a=30 mm (a/W=0.50), with 2 different thicknesses (5 mm and 10 mm) and 2 different notch radii (0.9 mm or 1.3 mm).  15 PLA plates with W=120 mm, a=30 mm (a/W=0.25), with 2 different thicknesses (5 mm, 10 mm, and 20 mm) and 2 different notch radii (0.9 mm or 1.3 mm).  12 PLA-Gr plates with W=60 mm, a=30 mm (a/W=0.50), with 2 different thicknesses (5 mm and 10 mm) and 2 different notch radii (0.9 mm or 1.3 mm).  15 PLA-Gr plates with W=120 mm, a=30 mm (a/W=0.25), with 2 different thicknesses (5 mm, 10 mm, and 20 mm) and 2 different notch radii (0.9 mm or 1.3 mm).

Figure 2: Geometry of the tested plates. ρ : notch radius; a: crack length; W: width; α : notch opening angle; L: length.

Figure 3: Experimental setup of two of the experiments: a) U-notch, a/W=0.25mm, notch radius=0.9 mm, thickness=10 mm; b) V notch, a/W=0.25 mm, thickness=5 mm.

325

Made with FlippingBook - professional solution for displaying marketing and sales documents online