S.E. Daguiani et alii, Frattura ed Integrità Strutturale, 66 (2023) 88-111; DOI: 10.3221/IGF-ESIS.66.05

(a) (b) Figure 14: SEM (a) and EDS (b) of hardened paste samples (control mixture) without Scms (Mix 01).

(a) (b) Figure 15: SEM (a) and EDS (b) of hardened paste samples containing 7.5% WGP as cement replacement (Mix 02).

(a) (b) Figure 16: SEM (a) and EDS (b) of hardened paste samples containing 7.5% GGBS as cement replacement (Mix 06).