observed with 1% of pseudo–ductile strain before the final failure and also laminates were almost free from free edge delamination as observed from Fig. 18 [41].
Figure 15: Schematic of hybridization of laminates [37]
Figure 16: a) Bearing stress-displacement curves of the SM-SM b) Bearing stress-displacement curves of the IM-HM [39]
Figure 17: The dispersed orientation stacking method[41]