Issue 65

H. Bahmanabadi et alii, Frattura ed Integrità Strutturale, 65 (2023) 224-245; DOI: 10.3221/IGF-ESIS.65.15

(a)

(b)

(c)

(d)

Figure 13: EDS mapping on the fracture surface of (a) AlSi at T max =250 °C, (b) AlSi at T max =350 °C, (c) AlSi_N_HT6 at T max =250 °C, and (d) AlSi_N_HT6 at T max =350 °C, under TMF testing with K TM =100% and t d =5 s.

240