Issue 63
A. Brotzu et alii, Frattura ed Integrità Strutturale, 63 (2023) 309-320; DOI: 10.3221/IGF-ESIS.63.24
Figure 7: XRD spectra confrontation: Ca-W TT 24h 1000°C (in blue) and Ca-W Lam TT 24h 1000°C (in red).
Figures 8: Tensile test curves of Ca-Cl (a) and Ca-W (b): yellow as cast (Type 1); green as cast+ heat treatment at 1000°C for 24 hours(Type 2); blue laminated (Type 3); red laminated + heat treatment at 1000°C for 24 hours.
316
Made with FlippingBook flipbook maker