A. Joshi et alii, Frattura ed Integrità Strutturale, 60 (2022) 158-173; DOI: 10.3221/IGF-ESIS.60.12

Figure 14: SEM Images showing fractured surface of Carbon-Jute Hybrid Composites (CJE) under Mode-I loading a) At Crack Initiation b) At Crack Propagation and (c) Mode-II fractured surface.

Figure 15: SEM Images of Carbon-Kenaf (CKE) Hybrid Composites during (a) Crack Initiation (b) Crack Propagation under Mode-I load and (c) Mode -II fractured surface.