appears more appropriate than others shapes when a two-dimensional simplified representation of the defects is requested [13]. The pores show a rounded shape sometime away any ellipse typically used for simplified fatigue assessment [8].
Figure 8: Three-dimensional model for a square-like crack (a=1 mm, L/a= 100, d/a=20).
Figure 9: Mesh and boundary conditions for a square-like crack of Fig. 8.
Figure 10: Stress ௠along the y-direction for the square-like crack of Fig. 4 for B on the symmetry axis