R. Maciel et alii, Frattura ed Integrità Strutturale, 48 (2019) 269-285; DOI: 10.3221/IGF-ESIS.48.28

identified. Each zone will have a different set of mechanical proprieties affecting the mechanical response of the entire joint, Fig. 13. The macroscopic images obtained for joints manufactured with three different load conditions (400, 425 and 450 kgf) are presented in the Figs. 14, 15 and 16 below:

Figure 14 : Hyb400-1: a) overall view; b) advancing side; c) retreating side

Figure 15 : Hyb425-1: a) overall view; b) advancing side; c) retreating side

Figure 16 : Hyb450-1: a) overall view; b) advancing side; c) retreating side