Issue 46

K.I. Tserpes et alii, Frattura ed Integrità Strutturale, 46 (2018) 73-83; DOI: 10.3221/IGF-ESIS.46.08

Figure 11 : Elastic modulus mapping, at 300 nm of displacement for a grid of 70  70 μ m 2 for MWCNT/PP 2 wt% specimen.

Figure 10 : Resistance to applied load mapping, at 300nm of displacement for a grid of 70  70 μ m 2 for MWCNT/PP 2 wt% specimen.

(a)

(b)

Figure 12 : (a) H / E and (b) H 3 / E 2 of MWCNT/PP 2 wt% specimen.

Figure 13 : Contact pressure (as resistance to applied load) mapping, at 300nm of displacement for a grid of 70 μ m 2 for polypropylene with 2 % CNTs.

80