A. Winkler et alii, Frattura ed Integrità Strutturale, 33 (2015) 262-288; DOI: 10.3221/IGF-ESIS.33.32
Figure 17. Typical morphology of injection moulded PA66.
Fig. 18 shows a microtome cut from a specimen made of POM. The difference in morphology is distinct, in that the spherulites are slightly elongated and that the injection moulding skin is much thicker (roughly 3 times).
Figure 18. Typical morphology of injection moulded POM