Crack Paths 2012
Figure 3. Fatigue initiators in bearing steel. Sizes of balls indicate ¥area of inclusion.
Multiple crack initiation
round a spherical cave for
oxide inclusion in 100Cr6
bearing steel fatigue
tested for 642 million
cycles at 735 M P a(R=-1).
Crack 3 lies on clearly
different plane and has
grown below 1 and 2,
thus causing retardation
and nonsymmetrical crack
growth.
Figure 4. Crack paths round the inclusion associated with the longest endurance.
1052